Page 62 - Read Online
P. 62
Page 76 Ragni et al. Extracell Vesicles Circ Nucleic Acids. 2026;7:73-93
EV staining
EV-containing conditioned media were either freshly processed (within 24 h) or thawed from -80 °C storage
and brought to 37 °C prior to staining. EVs were labeled with 10 µM CFSE [5(6)-Carboxyfluorescein
diacetate N-succinimidyl ester; Merk Life Science S.r.l., Milano, Italy], prepared fresh as a 5 mM stock
solution in dimethyl sulfoxide (DMSO) and incubated for 1 h at 37 °C in the dark. Following staining,
samples were concentrated and washed using centrifugal ultrafiltration units with a 100 kDa molecular
weight cutoff (Amicon® Ultra, MWCO 100 kDa; Merk Life Science S.r.l.). A maximum of 15 mL per run was
centrifuged at 4,000 × g to reduce volume to 500 µL. Two sequential washes with 14 mL PBS were performed
to remove unbound dye. Approximately 500 µL of concentrated, CFSE-labeled EVs were recovered and
processed for downstream applications.
Cell sorter calibration
Instrument (MoFlo Astrios EQ, Cell Sorter; Beckman Coulter, Brea, CA, USA), equipped with Blue 488 nm,
Yellow-Green 561 nm, Violet 405 nm, and Red 640 nm, was calibrated as previously described . The choice
[13]
of the instrument is due to its jet-in-air system, which interrogates particles with lasers in air, thereby
reducing sample stress. In addition, the presence of an obscuration bar minimizes background optical noise
and provides a reference signal that facilitates the detection of events close to the instrument’s sensitivity
limit. Finally, the dual-path Forward Scatter (FSC) configuration with two masks enables improved
discrimination between small and large particles. Briefly, after cell sorter set-up, side scatter (SSC) and FSC
parameters were calibrated using VER01A (189 nm) and VER01B (374 nm) Verity Shells hollow
organo-silica beads (Exometry, Amsterdam, The Netherlands), which exhibit light scattering properties and
refractive indices more similar to EVs than standard polystyrene beads. Background was assessed using
0.22 µm-filtered PBS, and instrument thresholds were optimized to minimize noise without compromising
detection of the smallest beads. Sorting conditions were optimized to minimize mechanical stress on EVs.
Instrument was optimized by reducing the sorting pressure associated with the nozzle size (70 µm nozzle
with a lower pressure of 35 psi instead of the standard 60 psi typically applied for this nozzle size).
EVs acquisition, sorting and purity check
The previously published procedure was followed . Briefly, the instrument background was first established
[13]
by acquiring 0.22 µm-filtered PBS on a SSC vs. FITC log plot at low flow rate (< 2,000 events/s) to minimize
electronic noise. Unstained conditioned medium was used to assess background fluorescence (~5,000
events/s), and CFSE-stained PBS served as a negative control to confirm specificity. CFSE-stained EVs were
acquired and gated into CFSE-positive and CFSE-negative populations using fluorescence and scatter
parameters. Gating strategy was based on comparison to unstained and PBS controls. Sorting was conducted
using a customized protocol with enabled parameters: 488-nm forward scatter 1 (FSC1), 488-nm forward
scatter 2 (FSC2), 488-nm side scatter (SSC), and 488-nm/513/26 channel (CFSE). Three dot plots were used
to define sorting gates: FSC1 vs. SSC, FSC2 vs. SSC and CFSE vs. SSC. Sorting was performed in Purify Mode
with a 1-2 drop envelope to ensure precise collection of gated events. After verifying the test stream and
stable flow rate, sorting was initiated and parameters were saved. Post-sorting, samples (5 µL diluted in 100
µL 0.22 µm-filtered PBS) were re-analyzed to confirm purity. Both CFSE-positive and CFSE-negative
populations were recorded to assess gating accuracy and sorting efficiency.
TEM analysis
Pre-sorted samples were diluted in 0.22 µm-filtered PBS to allow comparison with post-sorted samples based
on the number of nanoparticles per field. Briefly, samples were deposited onto formvar-carbon-coated grids
and incubated at RT for 10 min. Excess liquid was gently blotted using filter paper. Negative staining was
performed with 2% aqueous uranyl acetate for 10 min, followed by blotting to remove the excess stain. Grids
were air-dried at RT before imaging. Transmission electron microscopy (TEM) was conducted using a
TALOS L120C instrument (Thermo Fisher Scientific, Waltham, MA, USA) operating at 120 kV.